35%玻璃纤维增强和耐热注塑PA66级 A3WG7 BASF ® 巴斯夫 用于汽车燃油分配器和汽车变速箱组件
- 起订量 (千克)价格
- 25-500¥38 /千克
- 500-1000¥36 /千克
- ≥1000¥35 /千克
- 品牌:巴斯夫
- 货号:05131
- 发布日期: 2022-11-30
- 更新日期: 2024-11-16
产品详请
品牌 | 巴斯夫 |
货号 | 05131 |
用途 | 注塑 |
牌号 | A3WG7 |
型号 | A3WG7 |
品名 | PA66 |
外形尺寸 | 颗粒 |
生产企业 | 巴斯夫 |
是否进口 | 是 |
温馨提示:因橡塑行情波动太大,线上价格未能及时更新,更多详情及技术问题请来电咨询(微信同号)
Ultramid® A3WG7 | PA66-GF35 | BASF
Product Texts
Glass fibre reinforced and heat aging resistance injection moulding grade for industrial items such as gear wheels, solenoid valve housings, cable attachments, automotive fuel distributors and components for automotive gearshift.
Rheological properties | dry / cond | Unit | Test Standard |
Melt volume-flow rate, MVR | 20 / * | cm3/10min | ISO 1133 |
Temperature | 275 / * | °C | ISO 1133 |
Load | 5 / * | kg | ISO 1133 |
Molding shrinkage, parallel | 0.4 / * | % | ISO 294-4, 2577 |
Molding shrinkage, normal | 1.0 / * | % | ISO 294-4, 2577 |
Mechanical properties | dry / cond | Unit | Test Standard |
Tensile modulus | 11500 / 8500 | MPa | ISO 527-1/-2 |
Stress at break | 210 / 150 | MPa | ISO 527-1/-2 |
Strain at break | 3 / 5 | % | ISO 527-1/-2 |
Tensile creep modulus, 1h | * / 7450 | MPa | ISO 899-1 |
Tensile creep modulus, 1000h | * / 6600 | MPa | ISO 899-1 |
Charpy impact strength, +23°C | 95 / 105 | kJ/m2 | ISO 179/1eU |
Charpy impact strength, -30°C | 75 / - | kJ/m2 | ISO 179/1eU |
Charpy notched impact strength, +23°C | 14 / 22 | kJ/m2 | ISO 179/1eA |
Charpy notched impact strength, -30°C | 12 / - | kJ/m2 | ISO 179/1eA |
Thermal properties | dry / cond | Unit | Test Standard |
Melting temperature, 10°C/min | 260 / * | °C | ISO 11357-1/-3 |
Temp. of deflection under load, 1.80 MPa | 250 / * | °C | ISO 75-1/-2 |
Vicat softening temperature, 50°C/h 50N | 250 / * | °C | ISO 306 |
Coeff. of linear therm. expansion, parallel | 23 / * | E-6/K | ISO 11359-1/-2 |
Coeff. of linear therm. expansion, normal | 93 / * | E-6/K | ISO 11359-1/-2 |
Burning behavior at 1.5 mm nominal thickness | HB / * | class | IEC 60695-11-10 |
Thickness tested (1.5) | 1.5 / * | mm | IEC 60695-11-10 |
Yellow Card available | Yes / * | - | - |
Burning behavior at thickness h | HB / * | class | IEC 60695-11-10 |
Thickness tested (h) | 0.7 / * | mm | IEC 60695-11-10 |
Yellow Card available | Yes / * | - | - |
Oxygen index | 24 / * | % | ISO 4589-1/-2 |
Electrical properties | dry / cond | Unit | Test Standard |
Relative permittivity, 1MHz | 3.5 / 5.7 | - | IEC 62631-2-1 |
Dissipation factor, 100Hz | 200 / 3000 | E-4 | IEC 62631-2-1 |
Dissipation factor, 1MHz | 200 / 3000 | E-4 | IEC 62631-2-1 |
Volume resistivity | 1E13 / 1E10 | Ohm*m | IEC 62631-3-1 |
Surface resistivity | * / 1E10 | Ohm | IEC 62631-3-2 |
Electric strength | 40 / 34 | kV/mm | IEC 60243-1 |
Comparative tracking index | - / 450 | - | IEC 60112 |
Other properties | dry / cond | Unit | Test Standard |
Water absorption | 5 / * | % | Sim. to ISO 62 |
Humidity absorption | 1.6 / * | % | Sim. to ISO 62 |
Density | 1410 / - | kg/m3 | ISO 1183 |
Material specific properties | dry / cond | Unit | Test Standard |
Viscosity number | 145 / * | cm3/g | ISO 307, 1157, 1628 |
Rheological calculation properties | Value | Unit | Test Standard |
Ejection temperature | 195 | °C | - |
Test specimen production | Value | Unit | Test Standard |
Injection molding, melt temperature | 290 | °C | ISO 294 |
Injection molding, mold temperature | 80 | °C | ISO 294 |
Injection molding, injection velocity | 200 | mm/s | ISO 294 |